NACE-CIP2-001 無料問題集「NACE Coating Inspector Level 2」

You are the NACE Inspector on a project where a stationary floating structure is being coated and you notice a self-smoothing anti-fouling coating has been specified.
This is not a good choice because:

Generally for safety considerations, waterjetting hose connections use

Which concrete smoothing technique involves scrubbing a mixture of cement mortar over the concrete surface using ai cement sack, gunny sack, or sponge rubber float?

When performing a hardness test on a coating which has elastic properties the inspector is likely to likely to observe:

A reinforced coating is

Because a NACE Level 2 Inspector has been trained in specific destructive tests, it is up to the Inspector to decide if and when a destructive test is required.

You are working as the only in-house NACE Level 2 Inspector in a shop setting when an independent 3 rd party NACE Level 3 Inspector, representing the owner, presents you with a copy of a Non Conformance Report (NCR) he has written for a NACE2/SSPC SP 10 centrifugal blast which you had previously approved.
Your FIRST preferred course of action is to:

You are a NACE Level 2 in-house inspector working in a shop. Your in-house requires you to perform a sleeve test to test for soluble salts; however the 3 rd party NACE Level 3 inspector, the owner, has a san smart meter and has achieved a very different result and has rejected the pre-cleaning.
Your FIRST course of action is to:

In powder coatings, when the particles of powder begin to flow but are not fully liquid, they are in what stage?

On pipelines, which coating is identifiable by its distinct colors, usually light blue, green, or grey?